Crazing Cracks

Crazing Cracks BY DANIEL GREEN A crazed concrete surface contains a network pattern of very shallow, fine/hairline cracks. They do not penetrate much below the surface of the concrete. They rarely are more than 1/8” deep and are more noticeable...

Read more: Crazing Cracks

Delamination and Blisters

All surface defects in concrete are of concern.  To think that a short article such as this can address all of the causes and preventative measures for each defect is out of the question.  And this is certainly the case for delamination of concrete surfaces.
Delamination and Blisters BY DANIEL GREEN All surface defects in concrete are of concern. To think that a short article such as this can address all of the causes and preventative measures for each defect is out of the question. And this is...

Read more: Delamination and Blisters

Hodgson Concrete

  • Office: (334) 281-5141
  • Dispatch: (334) 281-0730
  • Fax: (334) 281-1911

Kirkpatrick Central

  • Office: (205) 423-2630
  • Dispatch: (205) 323-8394
  • Fax: (205) 423-2626

Kirkpatrick Northern

  • Office: (256) 582-3274
  • Dispatch: (256) 582-3274
  • Fax: (256) 582-3309

Walker Concrete

  • Office: (770) 506-7125
  • Dispatch: (770) 506-7125
  • Fax: (770) 507-9340
© Copyright 2019, ConcreteSouth.com
DBA: National Cement Company of Alabama, Inc.
A VICAT GROUP Company